Plastic CNC Machining Services
Advanced Plastic Materials
Premium engineering plastics for precision machining and rapid prototyping applications
ABS Plastic
Versatile thermoplastic with excellent impact resistance and machinability
- Impact strength: High
- Heat resistance: 80-100°C
- Surface finish: Excellent
Acrylic
Transparent thermoplastic with excellent optical clarity and weather resistance
- Light transmission: 92%
- UV resistance: Excellent
- Scratch resistance: High
Delrin (POM)
Low friction engineering plastic with excellent dimensional stability
- Friction coefficient: 0.2-0.4
- Wear resistance: Excellent
- Machinability: Outstanding
Nylon
High wear resistance engineering plastic for mechanical components
- Tensile strength: 70-90 MPa
- Abrasion resistance: Excellent
- Chemical resistance: Good
PEEK
High-performance thermoplastic for extreme temperature applications
- Max temp: 250°C
- Chemical resistance: Exceptional
- Strength-to-weight: Superior
Polycarbonate
Impact-resistant thermoplastic with excellent optical clarity
- Impact strength: 600-900 J/m
- Transparency: 88-90%
- Flame retardant: V-2
PTFE (Teflon)
Chemically inert fluoropolymer with exceptional non-stick properties
- Chemical resistance: Superior
- Friction coefficient: 0.04-0.10
- Max temp: 260°C
Technical plastics POM, PEEK and nylon: fast quote from your drawing
We machine the most requested engineering plastics to drawing: PEEK for high-temperature, high-load components (up to 260 °C, tolerances down to ±0.005 mm), POM/Delrin for low-friction gears, bushings and sliding parts, nylon for wear-resistant rollers, gears and structural parts. Certified raw material, first articles in 7–15 days, from 1 piece to volume production.
Send your technical drawing (PDF or STEP): a line-item quotation within 48 hours, certified material and tolerances confirmed by our programming team.
Quote in 48 hours — upload your drawingAdvanced Plastic Specifications
Technical specifications for engineering plastics and high-performance polymers
| Material | Tensile Strength | Max Temperature | Chemical Resistance | Applications |
|---|---|---|---|---|
| ABS | 40-50 MPa | 80-100°C | Good | Automotive, consumer products |
| Acrylic (PMMA) | 70-75 MPa | 70-95°C | Fair | Optical components, displays |
| Delrin (POM) | 60-70 MPa | 90-110°C | Excellent | Gears, bearings, bushings |
| Nylon (PA6/PA66) | 70-90 MPa | 80-120°C | Good | Wear parts, mechanical components |
| PEEK | 90-100 MPa | 250°C | Exceptional | Aerospace, medical, semiconductor |
| Polycarbonate (PC) | 60-70 MPa | 115-135°C | Good | Safety equipment, lenses |
| PTFE (Teflon) | 20-35 MPa | 260°C | Superior | Chemical processing, seals |
Advanced Manufacturing Capabilities
State-of-the-art precision plastic machining technologies for rapid prototyping and production
Ultra-High Precision
Achieve tolerances as tight as ±0.01mm with 5-axis CNC machining and in-process metrology
Automated Manufacturing
Robotic loading, unmanned machining cells, and AI-driven quality control for consistent production
Industry Certifications
ISO 9001:2015, ITAR registered, and RoHS compliant for medical & electronics
Get Your Plastic Parts Today
Upload your CAD files and receive instant quotes for custom plastic components
Get Instant Quote